Concrete
Future Potential Materials
Published
2 years agoon
By
admin
Asok Kr. Dikshit, Richa Mazumder, Sanjeev Kr. Chaturvedi and Lok Pratap Singh, National Council for Cement and Building Materials (NCCBM), discuss the themes of sustainable development in India’s cement sector, as the second piece from a three-part series.
It has been established by several researchers that different types of wastes/by-products of other industries can be utilised as alternative fuels and raw materials for cement production. Moreover, the circular economy is also supported by the production of blended cements, composite cements and utilising performance improvers (PI) (Kukreja et al. 2020). Portland Pozzolana Cement (PPC) and Portland Slag Cement (PSC), which uses fly ash and granulated blast furnace slag (GBFS) in the production of blended cements are not only beneficial for conservation of natural resources but also in lowering clinker factor in cement and reduction of CO2 emissions along with environmental sustainability. Moreover, various clays and LD slag are also in the lab scale R&D interfacial stage for application in the cement sector as raw materials.
Fly-ash
Fly ash is a by-product of burning pulverised coal in a coal-fuelled power plant. In particular, it is the unburned residue collected by either mechanical or electrostatic separators that is carried away from the burning zone in the boiler by the flue gases. The heavier unburned material drops to the bottom of the furnace and is termed bottom ash. Fly ash is a pozzolanic material consisting of finely-divided amorphous alumino-silicate with varying amounts of calcium. This when mixed with portland cement and water, will react with the calcium hydroxide released by the hydration of portland cement to produce various calcium-silicate hydrates (C-S-H) and calcium-aluminate hydrates. Technical assessment of fly ash is determined by physical and chemical characteristics which meet certain requirements.
The mineralogy and composition of fly ash is not constant and depends upon rather parent coal source, operating parameters and temperature of TPPs, the extent of coal preparation and cleaning, furnace design, usual climate storage and handling. The crystalline phases of the fly ash are determined by the mineralogical properties. Generally, fly ash has silica 40-60 per cent, alumina 20-40 per cent and ferrous 5–15 per cent by weight fractions (Singh et al. 2018). It mostly consists of mullite, quartz, magnetite, hematite and calcite as the common crystalline minerals (Šešlija et al. 2016). Fly ash is categorised into two classes – class F and class C, based on mineral composition and sources of coal.

Backfilling in the zinc lead mines.
In a few cement plants, fly ash is used as a raw mix component but, in most cases, fly ash is added to cement to produce Portland Pozzolana cement (PPC). Fly ash utilisation in the cement and construction industries can lower GHG emissions because such use offsets the emissions that result from mining activities and CO2 generation during cement production. Fly ash can decrease a higher percentage of the consumption of cement during construction. Out of the total fly ash generation, around 25 per cent is being utilised for cement industry (http://www.cea.nic.in/reports/others/thermal/tcd/flyash_201617.pdf). 33 per cent around still remains unutilised due to Geographical imbalanced and limitation of maximum 35 per cent fly ash, in PPC, as per IS:1489 (Part-I) (http://www.cea.nic.in/reports/others/thermal/tcd/flyash_201617.pdf).
In NCB various R&D work has been done on fly ash, some of which has been discussed below:
Evaluation of high-volume fly ash cements
The Indian standard specification IS: 1489 (Pt.I)-2015 for Portland Pozzolana Cement (PPC) permits 35 per cent (max) fly ash addition in PPC. In view of enhancing the use of fly ash in PPC in order to achieve resource conservation and environmental sustainability, NCB has taken up studies on preparation and evaluation of high volume fly ash cements (HVFAC) in line with European standard EN-197-1. Different approaches have been adopted to achieve desired strength development and other physical characteristics of HVFAC using fly ash and clinker materials available in different parts of India. Investigations have been carried out on performance evaluation of High-Volume Fly Ash Cement (HVFAC) up to 50 percent fly ash prepared by inter-grinding as well as separate grinding and blending of all the constituents. A similar strength development pattern was observed in the cement samples prepared with increasing percentage of fly ash with clinkers of different alite contents and maintaining same fineness level by inter-grinding as well as separate grinding and blending (Fig 5.). The effect of fineness levels was found to be more pronounced of HVFAC prepared with the clinker having higher alite.
Development of PPC based on fly ash and limestone
In this study, Portland composite cement blends were prepared (140 nos) with four types of clinker from different regions of India along with the regional available fly ash (15-35 per cent) and limestone (5, 7 and 10 per cent). The results depicted that the clinker quality plays an important role on performance of limestone and fly ash based composite cements. The mortar studies indicated Portland composite cements based on limestone and fly ash with 35 per cent replacement of clinker by fly ash and limestone (keeping limestone content upto 7 per cent in it). Hydration studies showed Monocarboaluminate (Ca4Al2O6 • CO3 • 11H2O) was found in the samples containing FA and LS, and the intensity of these peaks tend to be stronger when the amount of limestone is increased. Draft code formulation for submission to BIS is underway.
Development cement backfills pastes (CBP) using ultra-fine fly-ash and its evaluation
NCB has taken up several projects with Hindustan Zinc Limited in cement-based backfilling material/paste development. The target is for an application of the CBP as a cost-effective alternative to existing backfilling industrial solutions. Assimilation of fly-ash-an industrial waste: generated from a thermal power station along with other wastes generated from mining industries to produce CBP having the desired requirement, as per standing regulation, not only yields financial benefits of reduced consumption of cement whereby reducing carbon footprint; also, it allows utilisation of industrial waste whereby reducing the portion of material channelled to landfills. In the title project, the utiliSation of the ultra-fine fly ash for the preparation of CBP was studied at NCB, Ballabgarh. Based on the studies, NCB made a recommendation to HZL and is under consideration by the company. The studies’ results have
effectively achieved the target and are subject to application mine backfilling at SKE mines,
Udaipur, Rajasthan, India.
Investigations on utilisation of coarse fly ash (200-250 m2/kg)
Generation of fly ash in India is about 226 mtpa, out of which 26 per cent is being utilised in the cement industry. BIS allows fly ash of fineness above 250 m2/kg to be utilised for cement manufacturing. This investigation was carried out in NCB to study utilisation of coarser fly ash (200-250) in cement manufacture and to establish its technical suitability Investigations were carried out with fly ashes having the fineness below the specified BIS limit (250 m2/kg). The studies depicted that the coarser fly ash samples are meeting the mandatory requirements of IS 3812:2013, after grinding to 320±10 m2/kg. Studies on field wise samples indicated that the fineness is lower than 250 m2/kg at initial fields. However, grinding of these samples to 320±10 m2/kg resulted in improved characteristics conforming to IS 3812:2013.
Improving the reactivity of fly ash
The study carried out in NCB investigates the effect of mineral matter doping in the coal before combustion on its chemico-mineralogical constituents of the resultant ash. Different types of sintering aids were mixed with coal of different percentages. The ash prepared of the designed coal and dopants mixes in laboratory furnace at around 950°C. The resultant ash with and without dopants were evaluated for their chemico-mineralogy and microstructure characterisation using state of art instruments such as XRD, SEM and Optical Microscopy The mineralogical or crystalline compositions and glass content of doped ash samples shows better characteristics than the un doped sample. The addition of sintering aids may convert the crystalline content of silicate minerals into amorphous content and enhance the total amorphous content in the doped ash samples. Lime reactivity, and cement reactivity of doped ash samples shows better performance than the control sample.
Improving the properties of fly ash at higher fineness through mechanical activation
Fly ash has been established as the most sought-after material in cement, construction, and related building materials Industry. Enhancing the fly ash utiliSation in the manufacture of cement is identified as one of the key areas to mitigate the GreenHouse Gas emissions from cement industry. Owing to the poor reactivity of Indian fly ash, the cement industry is generally using activation methods to improve the properties of fly ash for enhanced use as a blending component in cement manufacturing. Among different methods of activation, mechanical activation is the most economic and effective way for improving the fly ash properties. Grinding of fly ash alone or along with clinker to the required fineness is a common practice in cement industry. Though increasing the fly ash content in cement has economic and environmental benefits, it results in decrease in the compressive strength values particularly at early ages.

Ground granulated blast furnace slag (GGBS)
In NCB, investigations were carried out on the mechanical activation of fly ash to the very high fineness values to see the effect of use of high fine fly ash on the properties of resultant cement. Though the physical properties and glass content values of the fly ash were found to be improving with the fineness, after a certain fineness some properties of fly ash such as lime reactivity (L.R.) and comparative compressive strength (C.C.S.) were found to be decreasing. Change in the microstructure of fly ash with increasing the fineness of fly ash was identified as the primary reason that is affecting the L.R. and C.R. values. Besides, increasing the fineness of clinker was found to be more beneficial than increasing the fineness of fly ash to absorb more fly ash in the cement manufacturing.
Blast furnace Slag is formed when iron ore, coke, and limestone or dolomite are heated at high temperatures. During this process, the limestone/dolomite acts as a flux and is chemically combined with the silicates and aluminates present in ore. Coke ash and the above products are mixed and produce blast furnace slag. This molten product can be cooled in several ways to form various types of slag, including ground granulated blast furnace slag (GGBS), which is rapidly cooled with large quantities of water to produce granules. GGBS is mixed with Portland cement clinker to make a blended cement known as Portland slag cement. Various phases are present in the slag including glass (supercooled liquid silicates), semi-glass, quartz, Ca-rich silicates, aluminosilicates, the presence of modified C3S and C2S phases, and in melilite, gehlenite, akermanite, merwinite, rankinite, pseudo wollastonite, monticellite, anorthite, forsterite, perovskite, spinel, etc. in minor amounts (Yildirim and Prezzi 2011). Currently India produced approx. 25 million tonnes BFS out of which 22 million tonnes of BFS is granulated and being consumed entirely in cement industry (Agarwal et al. 2017).

Steel slag and Cu slags are also used in cement manufacturing. In these types of slags, the morphometric complexity in the glass is typical, and semi-glass grains may behave as mineralisers. There is a direct effect of this slag on the formation of belite grains. However, these slags reduce the size of grains of both C3S and C2S if the pyro-processing system is disturbed. Steel slag can potentially replace conventional raw materials for clinker production owing to its relatively high content of oxides, such as CaO and Fe2O3. Additionally using steel slag as the raw material helps in the conservation of natural resources. Copper slag has a high Fe content and has been used as an iron adjustment material during the cement clinker production. Since the main composition of copper slag is vitreous FeSiO3, it has low melting point and could reduce the calcination temperature for cement clinker. Thus, the use of copper slag to replace iron powder as iron adjusting materials facilitates cement production, reduces or eliminates the need of mineraliser.
Some of the studies carried out in NCB on steel slag has been discussed below:
Utilisation of Granulated LD Converter Slag
Investigations were carried out in NCB to study the utilisation of granulated LD slag in the manufacture of cement and replacement of natural sand in cement mortars. The investigations revealed that LD slag could be gainfully utilised up to 5 per cent as performance improver in cement manufacture. The results indicated that compressive strength at 28-days improved up to 3.5 per cent as compared to that of control OPC without affecting the other parameters such as water requirement, setting time and soundness. Further, LD slag up to 40 per cent by weight could be added during the clinker grinding stage to manufacture cement blends. The compressive strength was found comparable to control OPC and PSC containing granulated BF slag. The investigations on use of LD slag as raw materials up to 4.25 per cent by replacing iron bearing additives in the raw mix revealed that good quality clinker could be produced at 1400 °C. The investigations on use of LD slag as replacement of natural sand in cement mortar established that LD slag could be gainfully utilised up to 100 percent. The replacement of natural sand in cement mortar also showed improved performance characteristics.
Utilisation of ladle furnace slag as a raw mix component
Exploration studies of Ladle Furnace Slag (LDF slag), which was a waste product from the steel industry were carried out in NCB as a raw mix component in manufacture of clinker to replace the laterite/red mud. Chemical and mineralogical investigations of LDF slag showed the presence of Fe2O3 in the range of 3 to 34 per cent, Al2O3 in the range of 14 to 33 per cent, SiO2 in the range of 3 to 21 per cent and CaO in the range of 33-51 per cent and calcium silicate, calcium aluminate, iron containing minerals etc. Computed mix designs were performed to optimise the raw materials with the similar potential minerals percentage, liquid content, AM, SM in the resultant clinker. LDF slag designed optimum compositions with the replacement level of 0.5 to 1.5 of laterite/red mud showed similar characteristics in terms of burnability as well as setting time, compressive strength and other physical characteristics.
Utilisation of Pet Coke Gasification Slag
A by-product slag, provided by M/s Reliance Industries Ltd, generated during the process of gasification of pet coke was investigated in NCB for its utilisation in the manufacture of OPC. In addition to CaO, SiO2, Al2O3, Fe2O3 and MgO, the slag also contains about 4 per cent vanadium. Investigations were carried out on the use of this slag as raw mix component in manufacture of Portland clinker. The burnability of cement raw mixes designed using 1-5 per cent pet coke gasification slag showed its mineralising effect, which was manifested through better lime assimilation and development of clinker mineral phases along with microstructure. The slag sample was also investigated for its suitability as performance improver in manufacture of OPC. The glass content in the sample was found to be 54 per cent and thus did not meet the requirement of Indian standard IS: 12089-1987. The physical characteristics of resultant cement were found to be comparable to its counterpart prepared using 5 per cent BF slag at all the ages.
Red mud
It is a byproduct of the aluminium industry. It contains numerous in situ mineralisers, which help to enhance quick phase formation in the clinker. However, the phases’ forms are different in shape and size. Red mud also affects the morphology of phases, which is fragmentation of alite and belite, thereby increasing the granulometry of phases. Tsakiridis et al. (2004) by addition of red mud into the raw meals assessed the feasibility of producing Portland cement clinkers. They used raw mix composition having 3.5 per cent Bayer-process red mud blended with 74.8 per cent limestone, 11.4 per cent schist, 3 per cent bauxite and 7.3 per cent Milos sand to prepare Portland cement clinkers. This raw meal is sintered at 1450°C and the produced clinkers mixed with the gypsum (5 per cent) to form final cement. It was observed that the addition of red mud in the raw mix resulted in a well-burnt clinker with a free lime content of 1.94 per cent at 1450°C. The chemical composition of the produced clinker was close to that of OPC clinker, and the incorporation of red mud residue at 3.5 per cent did not affect the mineralogical composition of the Portland cement clinker.
Use of red mud in cement production produces significant environmental and economic benefits such as natural resource management, promoting circular economy, lowering contamination of soil and groundwater, reducing landfill volume, cutting waste disposal costs, and decreasing the production cost of cement (Liu and Zhang, 2011)
Lime Sludge
It is waste mainly produced from the paper industry, other sources are fertiliser, sugar, carbide and soda ash industries. Lime sludge (LS) is generated by a kraft process through the chemical recovery section in a paper mill. The chemical composition of LS samples contains major CaO (52-55) per cent, SiO2 (1-4) per cent, Al2O3 and Fe2O3 make up less than 1 per cent by weight. Minor alkalis of Na2O, K2O and SO3 content are less than 1 wt per cent which is permitted as per Indian standard. al. has undertaken a study in which the lime sludge addition improved the burning ability of clinker which in turn reduced the temperatures for calcium carbonate (CaCO3) decomposition and liquid phase formation (Wei et al. 2014). Raw mix designed to manufacture cement clinker by using lime sludge and other cementitious raw materials, which has C3S, C2S, C3A, C4AF as clinker phase composition (Dikshit and Sahoo 2022).

Red Mud
The industrial LS is having the potential to be utilised as feasible raw material for cement preparation by replacing the limestone. Lime sludge can be used in 30-40 per cent in place of limestone because free lime content is observed to be low in the clinkers. Mineralogically C3S and C2S content is lying in the desired range and alite belite grain size are 27-34 µm and 14-23 µm respectively. NCB has validated lime sludge waste from paper and pulp industry in the cement manufacture application, which can bring sustainable development towards the environment as well as circular economy.
Use of Jarosite
In NCB, a study on Jarosite, a residual by-product generated from zinc industry during hydrometallurgical process containing predominantly Fe2O3, SO3, alkalies with small amounts of ZnO has been carried out. The constituent oxides present are known to contribute significantly in formation of clinker mineral phases and therefore, the Jarosite could be an effective mineraliser and activator in the manufacture of OPC clinker. The present study highlights the effect of addition of 0.5-2.0 per cent of typical Jarosite in cement raw mixes prepared with different grade limestone samples along with other conventional raw materials. The clinker parameters such as LSF, SM and AM were maintained in the range of 0.92, 2.07-2.18 and 1.01-1.14 respectively. Burnability studies on raw mixes showed increase in the rate of lime assimilation and rapid formation of clinker mineral phases in presence of Jarosite. The mineral phase developments and micro-structures of laboratory clinkers fired at 1400±5°C were found to be adequate in presence of optimum dose of 1.5 per cent Jarosite and were comparable to control clinker (without Jarosite addition) prepared at 1450±5°C. The physical performance of Ordinary Portland Cement thus prepared from above mineralised clinker showed performance comparable to control cement. As the Jarosite contains heavy elements, a leaching study was carried out by immersing 28-days hardened neat cement cubes in 500 ml distilled water over a period of 24 months. The leachates such as barium, cadmium, cobalt, chromium, copper, manganese, zinc, lead and strontium were found to be in negligible amounts.

Dried Lime sludge
Use of Marble Waste
Studies were carried out in NCB on the suitability of marble dust/slurry for use in cement manufacture as raw mix, as performance improver in OPC and in making Portland Limestone Cement (PLC). Performance evaluation of Portland Limestone Cement (PLC) composites prepared by blending of 15-30 per cent marble dust/limestone with OPC showed comparable strength development. Similarly, Ordinary Portland Cement samples containing 5 per cent marble dust collected from different marble clusters of Rajasthan also showed performance comparable to OPC containing 5 per cent limestone and conforming to IS requirement of CaCO3 =75 per cent laid down for limestone to be used as performance improver in OPC.
Phosphogypsum
Phosphogypsum is generated as a by-product during the manufacture of phosphoric acid. Approximately 4.5-5.5 tonnes of phosphogypsum is generated per tonne of phosphoric acid produced using wet process. Apart from the yearly generation of phosphogypsum, there is an additional issue of legacy stock of unutilised phosphogypsum of about 64.65 mt at various fertiliser plants accumulated over the years. In the manufacturing process of cement, phosphogypsum could be used as a replacement of natural gypsum which plays the role of a set retarder. Therefore, a project was taken up in NCB on investigations on utilisation of phosphogypsum in cement manufacturing.
Phosphogypsum along with mineral gypsum and clinker from different sources were collected for this study and their chemical, mineralogical and thermal characterisations were carried out. OPC blends were prepared using phosphogypsum and evaluated for chemical and physical properties. Initial results were found to be very encouraging. Further investigation is underway.
Technical feasibility of using FGD gypsum
Globally, Flue Gas Desulfurisation (FGD) systems have been installed in many thermal power plants in developed countries and FGD plants have been in operation in the US for 40 years. In India also the standards set by the MoEFandCC for coal-based thermal power plants came into force by which FGD systems need to be installed in them. Accordingly, a R&D project on technical feasibility of using FGD gypsum in cement manufacture is taken up in NCB. In this project, FGD gypsum is obtained from thermal power plants and other raw materials from cement plants. The FGD is characterised for their chemico-mineralogical properties. Mineralogical characterisation has been done by XRD and DTA. It clearly shows the presence of the Gypsum. The differential thermal analysis (DTA) indicates two endothermic peaks at 140°C due to the conversion of dihydrate to hemihydrate and a small hump at around 167°C due to conversion of hemihydrate to anhydrite of gypsum. In addition, an exothermic peak was recorded at 481°C, corresponding to the phase transformation of a CaSO4 to ? CaSO4. Chemical properties of Cement with both mineral and FGD gypsum clearly shows identical properties as per Indian Standards. The physical properties of cement Cement with both mineral and FGD gypsum clearly show comparable properties for all the properties, including normal consistency, setting time, and soundness. Furthermore, the compressive strength (CS) at 1D, 3D, 7D and 28 days for all samples with FGD gypsum shows similar performance compared to the control sample with mineral gypsum.
*The Authors wish to acknowledge the Director General of National Council for Cement and Building Materials (NCB) for giving permission for publication and DPIIT, Ministry of Commerce and Industry, GOI, through various R&D projects support financial
for sustainable development of cement Industry. The Authors also acknowledge all scientific and technical staff of NCB for cooperation through R&D work for sustainability of cement industry related projects.
**List of references will be featured in the concluding part of the series.

Concrete
The primary high-power applications are fans and mills
Published
2 days agoon
October 10, 2025By
admin
Alex Nazareth, Whole-time Director and CEO, Innomotics India, explains how plants can achieve both cost competitiveness and sustainability by lowering emissions, reducing downtime and planning for significant power savings.
As one of the most energy-intensive industries, cement manufacturing faces growing pressure to optimise power consumption, reduce emissions and improve operational reliability. Technology providers like Innomotics India are enabling this transformation by combining advanced motors, AI-driven digital solutions and intelligent monitoring systems that enhance process stability and reduce energy costs. From severe duty motors built for extreme kiln environments to DigiMine AI solutions that optimise pyro and mill operations, Alex Nazareth, Whole-time Director and CEO, Innomotics India, explains how the company is helping cement plants achieve measurable energy savings while moving closer to their sustainability goals.
How does your Energy Performance Contracting model typically reduce power consumption in cement plants—e.g., MWh saved?
Our artificial intelligence-based DigiMine AI Pyro and Mill solutions developed specifically for the cement industry, supports our customers in improving their process stability, productivity and process efficiency. In Pyro, this is achieved by optimising fuel consumption (Coal / AFR), reducing Specific Heat Consumption and reduction in emissions (CO2, SOx and NOx) through continuous monitoring of thermodynamics in pyro and recommending set-points of crucial parameters in advance for maintaining stable operations.
Within the mill, this is achieved by improving throughput, reduce energy / power consumption and maintaining stable operations on a continuous basis. Our ROI-based value proposition captures the project KPIs like reduction of coal usage, increase of AFR, reduction of specific heat consumption (Kcal / Kg), reduction of specific power consumption (KWH / tonne), reduction of emissions, etc., by a specific percentage. This gives clarity to our customers to understand the investment vis-à-vis savings and estimate the recovery time of their investment, which typically is achieved within one year of DigiMine AI Pyro and Mill solutions implementation.
What role do digitalisation and motor monitoring play in overall plant energy optimisation?
Motors are being used extensively in cement production, and their monitoring play crucial role in ensuring continuous operation of applications. The monitoring system can automatically generate alerts for any anomaly / abnormalities in motor parameters, which allows plant team to take corrective actions and avoid any major equipment damage and breakdown. The alerts help maintenance team to plan maintenance schedule and related activity efficiently. Centralised and organised data gives overview to the engineers for day-to-day activities. Cement is amongst the top energy intensive industries in comparison to other industries. Hence, it becomes critically important to optimise efficiency, productivity and up-time of plant equipment. Motor monitoring and digitalisation plays a vital role in it. Monitoring and control of multiple applications and areas
within the plant or multiple plants becomes possible with digitalisation.
Digitalisation adds a layer on top of OT systems, bringing machine and process data onto a single interface. This solves the challenges such as system silo, different communications protocol, databases and most importantly, creates a common definition and measurement to plant KPIs. Relevant stakeholders, such as engineers, head of departments and plant heads, can see accurate information, analyse it and make better decisions with appropriate timing. In doing so, plant teams can take proactive actions before machine breakdown, enable better coordination during maintenance activities while improving operational efficiency and productivity.
Further using latest technologies like Artificial Intelligence can even assist operators in running their plant with minimal requirement of human intervention, which allows operators to utilise their time in focusing on more critical topics like analysing data to identify further improvements in operation.
Which of your high-efficiency IEC low-voltage motors deliver the best energy savings for cement mills or fans?
Innomotics India offers a range of IEC-compliant low-voltage motors engineered to deliver superior performance and energy savings, particularly for applications such as cement mills, large fans, and blowers. Innomotics has the complete range of IE4 motors from 0.37kW to 1000kW to meet the demands of cement industry. The IE5 range is also available for specific requirements.
Can safe area motors operate safely and efficiently in cement kiln environments?
Yes, safe area motors are designed to operate reliably in these environments without the risk of overheating. These motors have ingress protection that prevents dust, moisture ingress and can withstand mechanical stress. These motors are available in IE3 / IE4 efficiency classes thereby ensuring lower energy consumption during continuous operation. These motors comply with relevant Indian as well as international standards.
How do your SD Severe Duty motors contribute to lower emissions and lower cost in heavy duty cement applications?
Severe duty motors enhances energy efficiency and durability in demanding cement applications, directly contributing to lower emissions and operational costs. With high-efficiency ratings (such as IE3 or better), they reduce power consumption, minimising CO2 output from energy use. Their robust design handles extreme heat, dust and vibration—common in cement environments—ensuring reliable performance and fewer energy losses.
These motors also lower the total cost of ownership by reducing downtime, maintenance and replacement frequency. Their extended service life and minimal performance degradation help cement plants meet sustainability targets, comply with emissions regulations and improve overall energy management—all while keeping production consistent and cost-effective.
What pump, fan or compressor drive upgrades have shown approximately 60 per cent energy savings in industrial settings and can be replicated in cement plants?
In the cement industry, the primary high-power applications are fans and mills. Among these, fans have the greatest potential for energy savings. Examples, the pre-heater fan, bag house fan, and cooler fans. When there are variations in airflow or the need to maintain a constant pressure in a process, using a variable speed drive (VSD) system is a more effective option for starting and controlling these fans. This adaptive approach can lead to significant energy savings. For instance, vanes and dampers can remain open while the variable frequency drive and motor system manage airflow regulation efficiently.
Concrete
We conduct regular internal energy audits
Published
2 days agoon
October 10, 2025By
admin
Shaping the future of low-carbon cement production involves integrating renewables, digitalisation and innovative technologies. Uma Suryam, SVP and Head Manufacturing – Northern Region, Nuvoco Vistas, gives us a detailed account of how.
In an industry where energy consumption can account for a significant portion of operating costs, cement manufacturers are under increasing pressure to adopt sustainable practices without compromising efficiency. Nuvoco Vistas has taken a decisive step in this direction, leveraging digitalisation, renewable energy and innovative technologies to drive energy efficiency across its operations. In this exclusive conversation, Uma Suryam, SVP and Head Manufacturing – Northern Region, Nuvoco Vistas, shares its approach to energy management, challenges of modernising brownfield plants and its long-term roadmap to align efficiency with India’s net-zero vision.
How has your company improved energy efficiency over the past five years?
Over the past five years, we have prioritised energy conservation by enhancing operational efficiency and scaling up renewable energy adoption. Through strategic fuel mix optimisation, deployment of cleaner technologies, and greater integration of renewables, we have steadily reduced our environmental footprint while meeting energy needs sustainably.
Technological upgrades across our plants have further strengthened efficiency. These include advanced process control systems, enhanced trend analysis, grinding media optimisation and the integration of solar-powered utilities. Importantly, grid integration at our key plants has delivered significant cost savings and streamlined energy management.
A notable milestone has been the expansion of our solar power capacity and Waste Heat Recovery Systems (WHRS). Our solar power capacity has grown from 1.5 MW in FY 2021–22 to 5.5 MW, while our WHRS capacity has increased from 44.7 MW to 49 MW, underscoring our commitment to sustainable energy solutions.
What technologies or practices have shown the highest energy-saving potential in cement production?
One of our most significant achievements in advancing energy efficiency has been the successful commissioning of a 132 KV Grid Integration Project, which unified three of our major manufacturing units under a single power network. This milestone, enabled by a dedicated transmission line and a state-of-the-art Line-In Line-Out (LILO) substation, has transformed our energy management and operational capabilities.
With this integration, we have substantially reduced our contract demand, eliminated power disruptions, and enhanced operational continuity. Supported by an optical fibre network for real-time communication and automation, this project stands as a testament to our innovation-led manufacturing excellence and underscores Nuvoco’s vision of building a safer, smarter, and sustainable world.
What role does digitalisation play in achieving energy efficiency in your operations?
Digitalisation plays a transformative role in driving energy efficiency across our operations. At Nuvoco, we are leveraging cutting-edge technologies and advanced digital tools to enhance productivity, optimise energy consumption and strengthen our commitment to sustainability and employee safety.
We are developing AI-enabled dashboards to optimise WHRS and kiln operations, ensuring maximum efficiency. Additionally, our advanced AI models evaluate multiple operational parameters — including fuel pricing, moisture content and energy output — to identify the most cost-effective fuel combinations in real time. These initiatives are enabling data-driven decision-making, improving operational excellence and reducing our environmental footprint.
What is your long-term strategy for aligning energy efficiency with decarbonisation goals?
As part of India’s climate action agenda, the cement sector has laid out a clear decarbonisation roadmap to achieve net-zero CO2 emissions by 2070. At Nuvoco, we view this as both a responsibility and an opportunity to redefine the future of sustainable construction. Our long-term strategy focuses on aligning energy efficiency with decarbonisation goals by embracing innovative technologies, alternative raw materials and renewable energy solutions.
We are making strategic investments to scale up solar power installations and enhance our renewable energy mix significantly by 2028. These initiatives are a key part of our broader vision to reduce Scope 2 emissions and strengthen our contribution to India’s net-zero journey, while continuing to deliver innovative and sustainable solutions to our customers.
How do you measure and benchmark energy performance across different plants?
We adopt a comprehensive approach to measure and benchmark energy performance across our plants. Key metrics include Specific Heat Consumption (kCal/kg of clinker) and Specific Power Consumption (kWh/tonne of cement), which are continuously tracked against Best Available Technology (BAT) benchmarks, industry peers and global standards such as the WBCSD-CSI and CII benchmarks.
To ensure consistency and drive improvements, we conduct regular internal energy audits, leverage real-time dashboards and implement robust KPI tracking systems. These tools enable us to compare performance across plants effectively, identify optimisation opportunities and set actionable targets for energy efficiency and sustainability.
What are the key challenges in adopting energy-efficient equipment in brownfield cement plants?
Adopting energy-efficient technologies in brownfield cement plants presents a unique set of challenges due to the constraints of working within existing infrastructure. Firstly, the high capital expenditure and relatively long payback periods often require careful evaluation before investments are made. Additionally, integrating new technologies with legacy equipment can be complex, requiring significant customisation to ensure seamless compatibility and performance.
Another major challenge is minimising production disruptions during installation. Since brownfield plants are already operational, upgrades must be planned meticulously to avoid affecting output. In many cases, space constraints in older facilities add to the difficulty of accommodating advanced equipment without compromising existing layouts.
At Nuvoco, we address these challenges through a phased implementation approach, detailed project planning and by fostering a culture of innovation and collaboration across our plants. This helps us balance operational continuity with our commitment to driving energy efficiency and sustainability.
Concrete
Enlight Metals Supplies 3,200 Tonne of Steel for Navi Mumbai Airport
The airport is set to become Asia’s largest air connectivity hub.
Published
2 days agoon
October 10, 2025By
admin
Enlight Metals has supplied 3,200 metric tonne of steel for the newly inaugurated Navi Mumbai International Airport, marking a major contribution to one of India’s largest infrastructure projects and reinforcing the company’s commitment to supporting national development.
The Navi Mumbai International Airport, developed under a Public-Private Partnership led by the Adani Group, was inaugurated today by Prime Minister Narendra Modi. The airport is set to become Asia’s largest air connectivity hub, enhancing regional connectivity, boosting economic growth, and expanding trade opportunities. Prime Minister Modi described the project as a “glimpse of Viksit Bharat,” highlighting its transformative impact on infrastructure and development in the region.
“The supply of 3,200 metric tonne of steel for this key project aligns with our focus on supporting critical infrastructure development through reliable and timely metal sourcing. Enlight Metals is committed to enhancing transparency and efficiency in the steel supply chain, contributing to projects integral to India’s growth objectives,” said Vedant Goel, Director, Enlight Metals.
Enlight Metals has implemented technology-driven solutions to strengthen supply chain efficiency, ensuring consistent availability of construction materials for large-scale projects nationwide. Its contribution to the Navi Mumbai International Airport underscores the company’s growing role in supporting India’s infrastructure development initiatives.
This milestone reflects Enlight Metals’ ongoing engagement in delivering quality materials and timely services for major national projects, further cementing its position as a reliable partner in India’s infrastructure sector

The primary high-power applications are fans and mills

We conduct regular internal energy audits

Enlight Metals Supplies 3,200 Tonne of Steel for Navi Mumbai Airport

World of Concrete India 2025 Showcases Global Expertise and Green Solutions

JSW Cement Opens Rs 1 Billion Plant in Odisha

The primary high-power applications are fans and mills

We conduct regular internal energy audits

Enlight Metals Supplies 3,200 Tonne of Steel for Navi Mumbai Airport

World of Concrete India 2025 Showcases Global Expertise and Green Solutions

JSW Cement Opens Rs 1 Billion Plant in Odisha
Trending News
-
Concrete4 weeks ago
Adani’s Strategic Emergence in India’s Cement Landscape
-
Concrete2 weeks ago
Cement Margins Seen Rising 12–18 per cent in FY26
-
Uncategorized1 week ago
Jindal Steel Commissions 5 MTPA Blast Furnace At Angul
-